Hemudur 18500 is a water-borne two-component polyamine cured epoxy primer containing zinc phosphate as corrosion inhibiting pigment. It cures to a strong and rust-preventing coat.
Complies with EU Directive 2004/42/EC, The Paints Directive on the limitation of volatile organic compounds: subcategory j.
As a general purpose primer on steel constructions (see REMARKS overleaf).
67°C [153°F]
Legislation | Value | % thinning, by volume |
---|---|---|
EU | 22 g/L [0.18 lb/US gal] | 140 |
US (coatings) | 22 g/L [0.18 lb/US gal] | |
US (regulatory) | 70 g/L [0.58 lb/US gal] | |
China | 22 g/L [0.18 lb/US gal] |
According to specific legislation, see details in the Explanatory Notes available at Hempel website, hempel.com or at your local Hempel website. VOC values may vary with shade, please consult the Safety Data Sheet, section 9. ªEU Directive 2004/42/CE.
Handle with care. Before and during use, observe safety labels on packaging and paint containers and follow all local and national safety regulations. Always consult Hempel’s Safety Data Sheet for this product along with the Product Data Sheet.
For professional use only.
Product code: 18500
Product components: Base 18509, Curing Agent 97710
Standard shade / code: Light grey 12170
Gloss: Semi-flat
Volume solids: 50 ± 2%
Specific gravity: 1.4 kg/L [11 lb/US gal]
Reference dry film thickness: 75 micron [3.0 mils]
Base 18509 : Curing Agent 97710 (2 : 3 by volume)
Stir well before use.
Fresh water
Hempel’s Cleaner 98701
Product temperature | Pot life |
---|---|
15°C [59°F] | 30 min |
20°C [68°F] | 60 min |
Tool | Thinning max vol. | Application parameters |
---|---|---|
Airless spray | 5% | Nozzle pressure: 150 bar [2200 psi] |
Nozzle orifice: 0.015-0.019″ | ||
Brush | 5% | Not Applicable. |
If brush or roller application is used, more coats will be necessary to achieve the specified dry film thickness. For brush or roller application use Hemucryl Brush Agent 99810. Spray data are indicative and subject to adjustment. Pressure is for a material temperature of 20°C [68°F].
Specification range | Low | High | Recommended |
---|---|---|---|
Dry film thickness | 50 micron [2.0 mils] | 120 micron [4.8 mils] | 75 micron [3.0 mils] |
Wet film thickness | 99 micron [4.0 mils] | 238 micron [9.5 mils] | 149 micron [5.9 mils] |
Theoretical spreading rate | 10 m²/L [407 sq ft/US gal] | 4.2 m²/L [171 sq ft/US gal] | 6.7 m²/L [273 sq ft/US gal] |
Overthickness must be closely controlled and never locally exceed 160 micron [6.4 mils] DFT. On irregular surfaces it is recommended to employ special care in avoiding over application.
Surface temperature | Surface dry | Hard dry | Fully cured |
---|---|---|---|
20°C [68°F] | min 120 | 4 hours | 7 days |
Determined for dry film thickness 75 micron [3.0 mils] at standard conditions, see Hempel’s Explanatory Notes for details.
Hempel’s specification supersedes any guidelines indicated in the overcoating table.
Quality name | 10°C [50°F] | 20°C [68°F] | 30°C [86°F] |
---|---|---|---|
Hemudur 18500 | Min: 10 h | Min: 4 h | Min: 2 h |
Max: Ext* | Max: Ext* | Max: Ext* | |
Hemucryl Enamel HI-Build | Min: 15 h | Min: 6 h | Min: 3 h |
Max: 17 d | Max: 7 d | Max: 3½ d |
*Ext: Depending on the actual exposure conditions, the coated surface is overcoatable for an extended period of time. Contact your local Hempel representative for advice.
Overcoating times are indicative for products of the same generic chemistry. Consult Hempel’s specification for more information.
Ambient temperature | Base | Curing Agent |
---|---|---|
25°C [77°F] | 12 months | 12 months |
Shelf life from date of production, when stored in original, unopened containers.
Thereafter, the product quality must be re-inspected.
Storage at elevated temperatures may reduce shelf life. For advice, please consult Hempel.
Dry film thickness | 1 µm | 1 mil |
---|---|---|
GWP (Global Warming Potential) | 9.5 g CO₂e/m² | 0.049 lb CO₂e/ft² |
The carbon footprint is for 1 square meter / square foot of surface area with a dry film thickness of 1 micron / mil.
The scope includes raw materials, in-bound transport to the Hempel factory, Hempel manufacturing processes, and any Volatile Organic Compounds emitted during and after the application of the product.
It is calculated based on the standard shade defined in this PDS.
Values may vary with shade.
Product Data Sheet – Hemudur 18500
Issued by Hempel A/S – May 2025
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations.