Hemucryl Primer HI-Build 18032 is a water-borne, acrylic dispersion paint with good anticorrosive properties. Especially suited for application by airless spray.
Complies with EU Directive 2004/42/EC, The Paints Directive on the limitation of volatile organic compounds: subcategory i.
As a primer in water-borne paint systems on interior and exterior steelwork in mildly to moderately corrosive environment.
May also be used as a primer in water-borne paint systems on hot dip galvanized steel, aluminium, and stainless steel in mildly corrosive environment.
Service temperature:
Flash point: 74°C [165°F]
Legislation | Value | Limit value, phase II (2010)ª |
---|---|---|
EU | 42 g/L [0.35 lb/US gal] | 140 |
US (coatings) | 54 g/L [0.45 lb/US gal] | – |
US (regulatory) | 118 g/L [0.98 lb/US gal] | – |
China | 42 g/L [0.35 lb/US gal] | – |
According to specific legislation, see details in the Explanatory Notes available at Hempel website, hempel.com or at your local Hempel website. VOC values may vary with shade, please consult the Safety Data Sheet, section 9.
ªEU Directive 2004/42/CE.
Handle with care. Before and during use, observe safety labels on packaging and paint containers and follow all local and national safety regulations.
Always consult Hempel’s Safety Data Sheet for this product along with the Product Data Sheet.
For professional use only.
*Issued by Hempel A/S – May 2025
Consult Hempel’s separate Surface Preparation Guidelines for more details.
Stir well before use.
Fresh water
Hempel’s Cleaner 98701
Tool | Thinning max vol. | Application parameters |
---|---|---|
Airless spray | 5% | Nozzle pressure: 130 bar [1900 psi] |
Nozzle orifice: 0.015-0.019″ | ||
Brush | 8% | Not Applicable |
If brush or roller application is used, more coats will be necessary to achieve the specified dry film thickness. For brush or roller application use Hemucryl Brush Agent 99810. Spray data are indicative and subject to adjustment. Pressure is for a material temperature of 20°C [68°F].
Specification range | Low | High | Recommended |
---|---|---|---|
Dry film thickness | 50 micron [2.0 mils] | 90 micron [3.6 mils] | 75 micron [3.0 mils] |
Wet film thickness | 117 micron [4.7 mils] | 210 micron [8.4 mils] | 175 micron [7.0 mils] |
Theoretical spreading rate | 8.6 m²/L [350 sq ft/US gal] | 4.8 m²/L [196 sq ft/US gal] | 5.7 m²/L [232 sq ft/US gal] |
Product may be specified in another film thickness than indicated depending on purpose and area of use.
This will alter spreading rate, drying and curing time and overcoating interval.
Overthickness must be closely controlled and never locally exceed 120 micron [4.8 mils] DFT.
On irregular surfaces it is recommended to employ special care in avoiding over application.
Relative Humidity:
Surface temperature | Surface dry | Through dry | Fully cured |
---|---|---|---|
20°C [68°F] | 60 min | 90 min | 7 days |
Determined for dry film thickness 75 micron [3.0 mils] at standard conditions, see Hempel’s Explanatory Notes for details.
Ambient temperature | Product shelf life |
---|---|
25°C [77°F] | 12 months |
Shelf life from date of production, when stored in original, unopened containers.
Thereafter, the product quality must be re-inspected. Storage at elevated temperatures may reduce shelf life.
For advice, please consult Hempel.
Dry film thickness | GWP (Global Warming Potential) |
---|---|
1 µm | 5 g CO₂e/m² |
1 mil | 0.026 lb CO₂e/ft² |
The carbon footprint is for 1 square meter / square foot of surface area with a dry film thickness of 1 micron / mil.
The scope includes raw materials, in-bound transport to the Hempel factory, Hempel manufacturing processes, and any Volatile Organic Compounds emitted during and after the application of the product.
It is calculated based on the standard shade defined in this PDS. Values may vary with shade.
Product Data Sheet – Hemucryl Primer Hi-Build 18032
Issued by Hempel A/S – May 2025
Document Version: 4/4
Source: https://www.hempel.com
Technical Guidelines and Explanatory Notes
Last accessed: 28 May 2025
Reference link: https://www.hempel.com/service-and-support/technical-guidelines
Note: Always consult the latest version of the Product Data Sheet and associated documents directly from Hempel’s official website to ensure accuracy and compliance with the most current recommendations.